How to Calculate the Tonnage of Die Casting Machine

The tonnage of die casting (or the clamping force - the tonnage of die casting machine can be converted to the clamping force of die casting machine. The conversion formula is shown at the end of the paper). a. Whether the die can be instal...

Causes of Cold-Shut and improvement measures

Q:What are the causes and solutions ofCold-Shut in Die-Castings? Appearance:Cold shut is a lapping that sometimes occurs where metal fronts join during the formation of solidified metal that sometimes occurs in the formation of die casting...

Causes of Die-Castings-Blisters and improvement measures

Q:What are the causes and solutions ofblisters in Die-Castings? Appearance: Blister is a surface defect or eruption caused by expansion of gas, usually as a result of heating trapped gas within the casting, or under metal which has been pla...

Causes of Die-Castings-Shrink and improvement measures

Q:What are the causes and solutions of shrink porosity in Die-Castings? Appearance: The surface of shrink porosity is dark and not smooth. Unlike gas porosity, shrink porosity consist of a series of irregular holes. How to lead to: 1. Shrin...

Causes of Die-Castings-Cracks and improvement measures

Q:What are the causes and solutions of cracks in Die-Castings? Appearance: The alloy matrix on the castings is broken or broken to form filamentous cracks, which have two kinds of penetration and non-penetration, and have a trend of develop...